What do sandpaper grit numbers mean? The CAMI and FEPA P scales, why P180 is not 180, coarse to very fine in numbers, how far to jump between grits, and which grit range does which job on metal and wood

A grit number is the mesh size used to sort the abrasive grain: the higher the number, the finer the grain and the finer the scratch it leaves. Two scales are in use in the United States. The CAMI scale (ANSI B74.18) has no prefix and is what most American bonded wheels and many coated discs carry; the FEPA scale carries a P prefix (P80, P180, P400) and is what most sanding belts, sheets and film discs carry today. The two match closely up to about 180 and then diverge, so P400 is about CAMI 320 and P1000 is about CAMI 500. In practice the work is done in ranges: 24 to 60 for stock removal and weld grinding, 80 to 120 for blending and shaping, 150 to 240 for finishing before paint, 320 and up for fine finishing and between coats. The usual rule for a grit sequence is to step up by no more than about 50 percent of the number at a time (80, 120, 180, 240) so each grit removes the scratches of the one before. The band lists the sanding discs, belts and sheets we stock by grit as the maker prints it.

Bayshore Safety. Industrial safety and PPE supplier since 2017. · Current as of November 2026 · ANSI B74.18, Grading of Certain Abrasive Grain on Coated Abrasive Material (the CAMI scale; summarized); FEPA Standard 43-1 (P-grit scale for coated abrasives; summarized); the 3M, Norton and CGW product data on this site (grit, backing, grain and size as printed); the 3M and Norton published grit comparison charts

Why two numbers that look alike are not the same. A 220 disc from one box and a P220 disc from another leave about the same scratch, but a 400 and a P400 do not: the P-scale number climbs faster past 180 because it is built on a tighter sieve tolerance. People who sand through a sequence that mixes the two scales get a visible jump in the finish. The cards below give the scale, the ranges and the sequence rule in the order the questions are asked.

Grit, question by question

Scale definitions are from ANSI B74.18 and FEPA 43-1; the ranges are the ones the abrasive makers print in their own selection charts.

What is the difference between CAMI and FEPA P grit?Both are sieve scales. CAMI (ANSI B74.18) numbers run 12 to 600 on coated abrasives and allow a wider spread of grain sizes within one grit; FEPA P (the European scale, written P12 to P5000) holds each grit to a tighter range. Up to about 180 the two scales match within a grit; above that the P number runs higher for the same grain size: P240 is about CAMI 220, P400 about 320, P600 about 360, P800 about 400, P1200 about 600. If a box says P, it is FEPA; no prefix on an American-made product means CAMI.
Which grit is coarse, medium, fine, very fine?The makers group them roughly as: extra coarse 24 to 36, coarse 40 to 60, medium 80 to 120, fine 150 to 220, very fine 240 to 400, extra fine 500 and up (micro grits, usually film or wet-or-dry paper). Non-woven abrasives use the words instead of numbers; that scale is in its own guide.
Which grit for grinding a weld flat?Stock removal on steel starts at 36 to 60 on a flap disc or fiber disc; 36 cuts fastest and leaves the deepest scratch, 60 leaves a surface that blends with less work afterwards. Ceramic grain at 36 or 40 is what the makers list for heavy weld removal; the grain guide linked below covers why.
Which grit before paint or primer?Paint and primer makers specify the scratch they want, commonly 80 to 120 under a high-build primer on bare metal and 180 to 320 between coats; the coating data sheet is the source for the number. Sanding finer than the coating calls for reduces adhesion rather than improving it.
How far can you jump between grits?The rule the makers print is to move up by no more than about one and a half times the previous number, so 40, 60, 80, 120, 180, 240, 320. Skipping from 60 to 220 leaves 60-grit scratches under a 220 finish that show when the part is painted or polished.
Does grit mean the same thing on a grinding wheel?A bonded wheel also carries a grit number (24, 36, 46, 60 are common) on the CAMI scale, printed as part of the marking code with the grain type and grade (hardness) letters. Reading that code is covered in the wheel label guide.
What grit for wood versus metal?The number means the same grain size on either; what changes is the range used. Rough wood starts at 60 to 80 and finishes at 180 to 220 before stain or clear coat; metal starts coarser (36 to 60) for removal and often ends finer (320 to 600) for a polished or brushed finish.
What is an open-coat versus closed-coat disc?Closed coat covers the backing fully with grain and cuts fastest on metal; open coat leaves spaces between grains so soft material (wood, paint, body filler) does not load the disc. The product name or data sheet states which; grit numbers are the same on both.

Grit in plain words

  • Higher number, finer grain, finer scratch. P in front means the FEPA scale.
  • Up to 180 the two scales agree; above it the P number runs higher for the same grain.
  • 24 to 60 removes metal; 80 to 120 blends; 150 to 240 preps for paint; 320 and up finishes.
  • Step grits by about one and a half times, not more.
  • The coating data sheet names the grit it wants under it.

Questions people ask

Is P180 the same as 180 grit?

Close: P180 and CAMI 180 are within a grit of each other. The scales separate above 180.

What is 1000 grit sandpaper used for?

Wet sanding clear coat and paint defects before polishing, and fine finishing on metal; it removes almost no material.

Which is coarser, 40 or 80 grit?

40 is coarser; the lower the number, the larger the grain.

What grit is a standard grinding wheel?

Most depressed-center grinding wheels are 24 to 36 grit; the number is in the marking code on the label.

Can you skip grits when sanding?

Each skipped step leaves scratches from the coarser grit; the makers’ charts step by about one and a half times.

What does the letter after the grit mean on a sheet?

On a bonded wheel the letter is the grade (hardness); on coated paper a letter such as A, C, D or E after the backing is the paper weight, not the grit.

The ratings, test results and standards shown here are the manufacturers' published values, reproduced as published. Nothing on this page is a recommendation by Bayshore Safety that any product is suitable for a particular task, hazard or workplace. Selecting safety products and protective equipment is the responsibility of the end user and the employer, based on their own hazard assessment and the regulations that apply to their work. Confirm every value on the manufacturer's own documentation before use.

Setting up a grinding bay or buying abrasives by the box?Call (925) 215-7337 or email us the wheel sizes, arbor, grit and the quantities and we will quote by the box and case with the part numbers listed. We sell nationwide.
All abrasives guides

© 2026 Bayshore Safety & Industrial Supplies, Inc. All rights reserved. This guide may not be copied or republished without written permission.

How to buyCard, purchase order or invoice terms; quotes on request; agencies and institutions welcome.
Live Service & SupportReal people who know the products, Monday to Friday 7:30am to 4pm Pacific. 925-215-7337
We DeliverWe ship nationwide. Parcel and LTL freight to job sites and businesses across the U.S.