Bayshore Safety & Industrial Supplies Guide
Tempil sticks, soapstone, paint markers and crayons: which mark stays on hot or oily metal, and how temperature sticks work? Melting-point temperature indicators and reading them, preheat and interpass checks under AWS D1.1, soapstone holders and flats, solid paint markers vs liquid paint markers vs permanent ink, welding crayons and lumber crayons, low-chloride markers for stainless and nuclear work, and removal
Two different things get called a marker in a welding shop: tools that mark the steel, and tools that tell you how hot it is. A temperature indicating stick (Tempilstik is the common brand) is a crayon of a material calibrated to melt at one temperature, 100 to 2,500 °F in steps; the welder strokes the steel and when the mark changes from a dry chalk line to a wet, glossy smear the metal has reached that temperature, which is how preheat and interpass temperatures required by AWS D1.1 and welding procedures are checked without a pyrometer (two sticks bracket a range: one that melts at the minimum, one that stays dry at the maximum). Temperature labels and lacquers do the same for parts that cannot be stroked. For marking: soapstone (talc) is the layout tool that survives heat, is seen through a welding lens, wipes off, and does not contaminate a weld; it comes as flat and round sticks in a metal holder. Solid paint markers (Markal B and Paintstik) are paint in stick form that marks rough, rusty, wet and oily steel and stays through weather and handling; liquid paint markers (valve-action) give a finer permanent line; permanent ink markers fade on hot or oily metal; welding crayons and lumber crayons are wax and mark wood, concrete and cold steel but melt off hot work. Stainless, nickel and nuclear work require markers certified low in chlorides, halogens, sulfur and low-melting metals (lead, zinc, copper) because those cause corrosion and cracking at weld temperature, and the makers print the certification. The band lists the temperature sticks, soapstone, holders, paint markers and crayons we stock.
Why a crayon is a code instrument. A welding procedure says preheat to 150 °F, or 225, or hold interpass below 500, and the inspector asks how the welder knew. The temperature stick is the accepted answer in D1.1 and the shop; it costs a few dollars and reads to a few degrees. The marking tools are the other half of the same bench, and the one rule that catches people is the chloride rule on stainless. The cards cover the sticks, then each marking tool, then the contamination rule and removal.
Temperature sticks and markers, question by question
Temperature use follows the code and the maker’s instructions; marker surface and temperature claims are the makers’.
In plain words
- A temperature stick melts at its number: dry mark means not there yet, wet smear means reached. Stroke as the part heats.
- Two sticks bracket preheat and interpass; D1.1 says check through the thickness, away from the flame.
- Soapstone for layout: seen through the lens, survives the arc, wipes off, contaminates nothing.
- Solid paint marker for rusty, wet, oily steel that must stay marked; liquid paint marker for fine permanent lines; ink fades.
- Wax crayons for wood, concrete and cold steel; they melt off hot work.
- Stainless and nuclear: certified low-chloride markers only, and remove them before service.
Questions people ask
How do you use a Tempilstik?
Stroke it on the part as it heats; a dry chalk mark means below its temperature, an instant wet smear means the rating has been reached.
How accurate are temperature indicating sticks?
The maker rates them at about plus or minus 1 percent of the stated temperature.
Why do welders use soapstone?
It marks steel with a line visible through the lens, survives the arc, contaminates nothing and wipes off.
What marker works on oily or rusty metal?
A solid paint marker (Paintstik type); soapstone and ink do not mark through oil.
What is a low-chloride marker?
A marker certified below stated chloride, halogen, sulfur and low-melting-metal limits for stainless, nickel and nuclear work.
Can you check preheat with one stick?
One stick confirms the minimum was reached; a second stick at the maximum interpass confirms it was not exceeded.
Related guides
Welding electrode numbers explainedThe rods whose procedures set the preheatAbrasives for stainless, aluminum and steelContamination on stainless from the abrasive sideLevels, squares and layout toolsThe rest of the layout kitStainless steel welding fumesThe respirator side of stainless weldingWelding lens shade chartSeeing the soapstone line through the lensThe ratings, test results and standards shown here are the manufacturers' published values, reproduced as published. Nothing on this page is a recommendation by Bayshore Safety that any product is suitable for a particular task, hazard or workplace. Selecting safety products and protective equipment is the responsibility of the end user and the employer, based on their own hazard assessment and the regulations that apply to their work. Confirm every value on the manufacturer's own documentation before use.
© 2026 Bayshore Safety & Industrial Supplies, Inc. All rights reserved. This guide may not be copied or republished without written permission.