Skip to main content
Home › Guides › Welding and cutting › Welding rod numbers
Guide · Welding and cutting · AWS A5.1 electrode classification, E6010 to E7018, rod storage and ovens

Bayshore Safety & Industrial Supplies Guide

What do welding rod numbers mean? E6010, E6011, E6013, E7018 and how rods are stored: the AWS A5.1 code (tensile strength, position, coating and current), what each common rod is used for, polarity, rod diameter by metal thickness and amperage, low-hydrogen storage and rod ovens, and the D1.1 exposure limits

A stick electrode number is an AWS A5.1 classification and it reads in four parts. E means electrode. The next two (or three) digits are the minimum tensile strength of the weld metal in thousands of psi: 60 for 60,000 psi, 70 for 70,000. The next digit is position: 1 for all positions (flat, horizontal, vertical, overhead), 2 for flat and horizontal fillet only, 4 for all positions with vertical down. The last digit, read together with the one before it, names the coating and the current: E6010 is a high-cellulose sodium coating for DC electrode positive only, the deep-penetrating root pass and pipe rod; E6011 is high-cellulose potassium for AC or DC, the same arc on an AC buzz box; E6013 is a high-titania potassium rutile rod for AC or DC, a soft arc and easy slag for sheet and general repair; E7018 is a low-hydrogen iron powder rod for AC or DC positive, the structural and code rod with the smooth bead, which must be kept dry; E7014 and E7024 are iron powder fast-fill rods for flat work. Suffixes add things (E7018-1 for toughness, H4R for hydrogen control and moisture resistance). Rod diameter (3/32, 1/8, 5/32, 3/16 inch) follows metal thickness and sets the amperage range the maker prints on the box (a 1/8 inch E7018 runs about 110 to 165 amps, a 1/8 inch E6010 about 75 to 125). Storage is where E7018 differs from the others: its coating absorbs moisture that puts hydrogen into the weld and cracks it, so AWS D1.1 requires low-hydrogen rods kept in a holding oven at 250 to 300 °F once the hermetic can is opened, limits exposure to the air to 4 hours for E70XX (less at higher strengths), and allows one re-bake at 500 to 800 °F per the maker; cellulose rods (E6010, E6011) are not oven-dried, because the coating needs its moisture. The band lists the electrodes, rod ovens and holders we stock by classification and size.

Bayshore Safety. Industrial safety and PPE supplier since 2017. · Current as of November 2026 · AWS A5.1/A5.1M, Specification for Carbon Steel Electrodes for Shielded Metal Arc Welding (classification system; summarized); AWS D1.1/D1.1M, Structural Welding Code, Steel, clause on low-hydrogen electrode storage and exposure (summarized); the Lincoln Electric, Hobart and ESAB electrode data sheets (amperage ranges, polarity, storage) for the rods on this site; the welding electrode and rod oven product data on this site (classification, diameter, package and oven temperature as printed)

Why the last two digits matter more than the first two. Most rods on a jobsite are 60 or 70 series, so the strength number rarely decides anything; the coating digits decide whether the rod runs on the machine you have (AC or DC), how it penetrates, what the slag does, and whether the rod has to live in an oven. E7018 is the rod the codes ask for and the rod people ruin by leaving the can open. The cards decode the number, run through the common rods, size and amperage, polarity, and the storage rules.

Electrode numbers, question by question

The classification is AWS A5.1; amperage ranges are the makers’ and vary by brand; storage limits are AWS D1.1 and the makers’.

How do I read E7018?E: electrode. 70: minimum 70,000 psi tensile strength of the deposited weld metal. 1: all positions. 8, read with the 1 as 18: low-hydrogen potassium coating with iron powder, AC or DC electrode positive. So E7018 is a 70 ksi, all-position, low-hydrogen rod. E6010: 60 ksi, all positions, 10 = high-cellulose sodium, DC positive only. E6011: same with potassium, AC or DC. E6013: 13 = high-titania potassium, AC or DC either polarity. E7024: 2 = flat and horizontal only, 24 = iron powder titania, high deposition. The three-digit strengths (E11018) are the same system at higher strength.
What is each common rod used for?E6010: deep penetration, fast-freezing puddle, forceful arc that digs through rust, paint and mill scale; open-root pipe and plate roots, vertical-down, dirty steel; DC machines only. E6011: the AC version of 6010 for the same work on a transformer machine, slightly less penetration. E6013: soft arc, shallow penetration, easy slag, smooth bead; sheet metal, thin tube, general repair, beginners’ rod; AC or DC. E7014: iron powder, easy running, more fill than 6013; general fabrication. E7018: low-hydrogen, smooth strong ductile welds, the rod structural codes and most procedures require on thicker and higher-strength steel; harder to start and restart, needs clean steel and dry storage. E7024: very high deposition for flat and horizontal fillets in production. E6022 and E7028 are specialty flat rods; the data sheet governs.
What rod diameter and amperage?Diameter follows the metal: 3/32 inch for sheet to about 1/8 inch; 1/8 inch for 1/8 to 1/4 inch and the general rod; 5/32 for 1/4 inch and up; 3/16 and 7/32 for heavy plate. The maker prints the amperage range on the box for each diameter and classification; typical mid-ranges: E6010 and E6011 at 3/32, 40 to 85 amps; 1/8, 75 to 130; 5/32, 110 to 165. E6013 at 1/8, 80 to 130. E7018 at 3/32, 70 to 110; 1/8, 110 to 165; 5/32, 150 to 220. Out-of-position work runs toward the low end; the rule of thumb (one amp per thousandth of diameter) gets close for 1/8 inch rods and the data sheet does the rest.
AC, DCEP or DCEN?DCEP (electrode positive, reverse polarity): the standard for E6010 (which runs only on it), E7018 and most rods; deepest penetration. DCEN (electrode negative, straight): shallower penetration, higher deposition; some E6013 and E7014 work and sheet metal. AC: the transformer buzz-box current; E6011, E6013, E7014 and AC-rated E7018 run on it, E6010 does not, and AC resists arc blow on magnetized steel. The box states the current and polarity; running a rod on the wrong one gives a spitting, unstable arc.
Why does E7018 have to stay dry?The low-hydrogen coating is made with minimal moisture so the weld picks up little hydrogen; hydrogen in the weld metal causes underbead and delayed cracking, especially in thick, restrained and higher-strength steel, which is exactly where E7018 is specified. Once the hermetically sealed can is opened the coating draws moisture from the air. AWS D1.1 therefore requires E70XX low-hydrogen rods to go into a holding oven at 250 to 300 °F (120 to 150 °C) and limits exposure to the air to 4 hours for E70XX (2 hours for E80XX, 1 hour for E90XX, 30 minutes for E100XX and E110XX) before they go back in the oven; rods exposed longer are re-baked once at 500 to 800 °F for the time the maker states, then held at 250 to 300; wet or twice-baked rods are discarded. H4R and moisture-resistant coatings extend the exposure under the code. Cellulose rods (E6010, E6011) are never oven-stored: their coating is designed to contain moisture, and drying it ruins the arc.
What is a rod oven, and what are the sizes?Portable rod ovens (5 and 10 lb, 120 volt, with a thermostat set around 250 to 300 °F) hold a day’s E7018 at the welder; bench and floor ovens (50 to 350 lb) hold stock at the same temperature; re-bake ovens reach 800 °F for reconditioning. Rod canisters and dry-rod tubes carry a few rods from the oven to the joint and are not a substitute for the oven past the exposure time. The oven thermometer is checked, and the oven is for low-hydrogen rods only; cellulose, rutile and aluminum rods are stored dry at room temperature in sealed containers.
Stainless, cast iron, hardfacing and aluminum rodsThe same numbering idea applies in other AWS specifications: E308L-16 and E309L-16 (A5.4) for stainless, with the last two digits again naming coating and current; ENi-CI and ENiFe-CI (A5.15) for cast iron; hardfacing rods by alloy; E4043 (A5.3) for aluminum stick welding. Each has its own storage note (stainless and nickel rods are kept dry and often oven-held; the makers state it) and its own amperage table.
What PPE and rules apply to stick welding?Shade 10 to 14 by amperage under the 1910.252(b)(2)(ii)(I) table and the shade chart guide; leather gauntlet gloves, FR or leather jacket or sleeves and apron, a cap under the helmet, safety glasses under the hood for chipping slag; fume control per the welding fume guides, with the hexavalent chromium rule for stainless; the electrode removed from the holder when the machine is left, dry gloves and insulated footing in wet conditions (1910.254(d) and 1926.351), and a hot work permit and fire watch under 1910.252(a). Rod stubs are hot and go in a metal can.

In plain words

  • E, strength in ksi, position digit, then two digits for coating and current.
  • 6010 digs and roots on DC; 6011 is its AC twin; 6013 is the soft general rod; 7018 is the code rod and must stay dry; 7024 fills flat.
  • Diameter follows metal thickness; amperage comes off the box.
  • DCEP for most; AC for buzz boxes and arc blow; the box says which.
  • 7018 lives in a 250 to 300 degree oven once the can is open; 4 hours out, one re-bake, then the trash.
  • Cellulose rods never go in the oven.

Questions people ask

What does the 70 in 7018 mean?

A minimum tensile strength of 70,000 psi for the deposited weld metal under AWS A5.1.

What is the difference between 6010 and 6011?

6010 has a sodium cellulose coating and runs on DC positive only; 6011 has a potassium coating and runs on AC or DC with a similar deep-penetrating arc.

Can 7018 be run on AC?

Rods marked E7018 AC or carrying the AC rating can; the box states the current. DC electrode positive is the standard.

How long can 7018 be out of the oven?

AWS D1.1 allows 4 hours for E70XX low-hydrogen rods before they return to a 250 to 300 °F oven; one re-bake at 500 to 800 °F is permitted.

Should 6010 rods be stored in an oven?

No; cellulose coatings need their moisture, and oven drying ruins the arc. Store them dry at room temperature.

What amperage for a 1/8 inch 7018?

The makers list about 110 to 165 amps; the box range for the brand governs.

The ratings, test results and standards shown here are the manufacturers' published values, reproduced as published. Nothing on this page is a recommendation by Bayshore Safety that any product is suitable for a particular task, hazard or workplace. Selecting safety products and protective equipment is the responsibility of the end user and the employer, based on their own hazard assessment and the regulations that apply to their work. Confirm every value on the manufacturer's own documentation before use.

Setting up a welding shop or restocking consumables?Call (925) 215-7337 or email us the processes, the machines and the quantities and we will quote tips, consumables, cable and accessories by the box with the part numbers listed. We sell nationwide.
All welding and cutting guides

© 2026 Bayshore Safety & Industrial Supplies, Inc. All rights reserved. This guide may not be copied or republished without written permission.

How to buyCard, purchase order or invoice terms; quotes on request; agencies and institutions welcome.
Live Service & SupportReal people who know the products, Monday to Friday 7:30am to 4pm Pacific. 925-215-7337
We DeliverWe ship nationwide. Parcel and LTL freight to job sites and businesses across the U.S.